Author: Jennifer Hritz 
Type: General 
Category: Optical Contacting 
Subject: Cause of improved bond: time or pressure 

Before jumping to conclusions based on my previous results, I wanted to check that it was indeed heat and pressure, not time, that led to the bonds improving.

I prepared 4 samples, all with my standard pressing technique (which still leaves room for improvement). 2 samples will simply be left to sit undisturbed, and the other 2 will be left under both (rectangular and cylindrical) weights. I will check these in roughly 24 hours, just like the last test.

The 2 slides on the right are the ones under the weights.

Attachment 1: before_time_on_left_pressure_on_right_PXL_20221003_061828860.MP.jpg  504 kB  Uploaded Mon Oct 3 00:33:21 2022  | Hide | Hide all
before_time_on_left_pressure_on_right_PXL_20221003_061828860.MP.jpg
Attachment 2: set_up_time_vs_pressure_PXL_20221003_062018249.MP.jpg  4.543 MB  Uploaded Mon Oct 3 00:33:35 2022  | Hide | Hide all
set_up_time_vs_pressure_PXL_20221003_062018249.MP.jpg
Attachment 3: in_progress_time_vs_pressure_PXL_20221003_062117715.MP.jpg  3.915 MB  Uploaded Mon Oct 3 00:34:30 2022  | Hide | Hide all
in_progress_time_vs_pressure_PXL_20221003_062117715.MP.jpg