40m QIL Cryo_Lab CTN SUS_Lab TCS_Lab OMC_Lab CRIME_Lab FEA ENG_Labs OptContFac Mariner WBEEShop
  OMC elog  Not logged in ELOG logo
Message ID: 90     Entry time: Mon Apr 1 10:28:03 2013
Author: Koji 
Type: Mechanics 
Category: General 
Subject: Additional UV blast for the top surface 

[Koji, Lisa, Jeff, Zach]

Jeffs concern after talking with the glue company (EMI) was that the UV blast for the top side was not enough.

First we wanted to confirm if too much blasting is any harmful for the glue joint.

We took a test joint of FS-FS with the UV epoxy. We blasted the UV for 1min with ~15mm distance from the joint.
After the observation of the joint, we continued to blast more.
In total, we gave additional 5min exposure. No obvious change was found on the joint.

P3283483.JPG

Then proceed to blast the OMC top again. We gave 1 min additional blast on each glue joint.

 P3283459.jpg P3283473.JPG

ELOG V3.1.3-