Entry  Wed Aug 3 15:36:57 2016, Steve, Update, SUS, Ni plated magnets & epoxy ordered 
    Reply  Fri Aug 5 09:38:12 2016, Steve, Update, SUS, SOS sus wire ordered 0.0017.jpg0.0017spec.jpg
       Reply  Mon Aug 15 14:29:32 2016, Steve, Update, SUS, SOS sus wire ordered 
          Reply  Mon Aug 15 14:34:33 2016, ericq, Update, SUS, SOS sus wire ordered 
          Reply  Wed Aug 17 22:09:04 2016, rana, Update, SUS, SOS sus wire ordered 
       Reply  Thu Aug 18 15:16:09 2016, Steve, Update, SUS, SOS sus wire is in 0.0017new.jpg
          Reply  Wed Nov 30 14:53:56 2016, Steve, Update, SUS, new sus wire stored in N2 filled dessicator dessicatorC.jpgwireN2c.jpg
Message ID: 12410     Entry time: Mon Aug 15 14:34:33 2016     In reply to: 12409
Author: ericq 
Type: Update 
Category: SUS 
Subject: SOS sus wire ordered 

We have indeed seen numerous tarnished/rusty points along the wires, and just tried to choose lengths free of any of these. I wonder if this can explain the brittleness/ease with which we've been breaking it. My feeling is that we should use the newer wire if feasible.